Here is a comparative table of Ni-Fe-Cr based Incoloy nickel alloys (600, 601, 625, 617, 817) and Inconel mesh:
Alloy/Material |
Chemical Composition (Main Elements and Contents) |
Performance Characteristics |
Application Fields |
Incoloy 600 |
Ni 32%-44%, Cr 14%-21%, Fe 21%-31%, with trace elements such as Ti and Al |
– High strength and good plasticity at room and high temperatures |
Aerospace (high-temperature components of engines), energy (gas turbines, boilers), chemical industry (high-corrosion equipment/pipelines), high-temperature furnaces |
Incoloy 601 |
Ni 58%-63%, Cr 21%-25%, Fe balance, Al 1.0-1.7, C≤0.10, Mn/Si≤1.0, S≤0.015 |
– Outstanding high-temperature oxidation resistance |
High-temperature furnace components, heat treatment equipment, chemical processing equipment (scenarios requiring resistance to high-temperature oxidation and corrosion) |
Incoloy 625 |
Ni balance, Cr 20%-23%, Mo 8%-10%, Nb+Ta 3.15-4.15, Fe≤5.0, Al 0.4, C/Mn/Si≤0.5, S≤0.015 |
– Excellent resistance to pitting, crevice corrosion, and stress corrosion cracking |
Aerospace (engine components), marine engineering (offshore platform pipelines), petrochemical industry (reaction vessels), nuclear industry (reactor components) |
Incoloy 617 |
Ni balance, Cr 20-24%, Co 10-15%, Mo 8-10%, Al 1.0-1.7, C 0.05-0.15, Mn/Si≤1.0, Fe≤3.0 |
– Ultra-high temperature (up to 1200℃) oxidation and hot corrosion resistance |
Industrial furnaces, gas turbines, aerospace engines, nuclear reactors (high-temperature and high-stress service conditions) |
Incoloy 817 |
Ni balance, Cr 22-25%, Mo 12-14%, W 2.5-3.5%, C 0.05-0.15, Mn/Si≤1.0, Fe≤3.0, Co≤3.0 |
– Exceptional resistance to carburization, oxidation, and sulfidation at high temperatures (up to 1150℃) |
Chemical processing (high-temperature reactors), heat treatment equipment, coal gasification systems, aerospace components exposed to complex high-temperature media |